The bonding performance between the restorative materials and cements were material type-dependent and surface treatment had a large effect on the bond strength. Within the limitations of the study, the use of both U200 and TheraCem may be suggested if Z-prime was applied to intaglio surfaces of VE. The cementation of LU using TheraCem is suitable after HF acid conditioning of the restoration surfaces.